All data is for information only------(Home) | |
---|---|
PRODUCT DATA of AISI 430 |
Material | AISI 430 |
Product Datasheet | Carpenter 430 AK steel 430_Data_Sheet |
General Information | Ferritic stainless steel |
Chemical Composition | Fe-17Cr-0.15C |
EXPERIENCE IN PRACTICE |
---|
Equivalent Designations | 1.4742'; X10CrAl18; 430 S15; Z10CAS18; X8Cr17 |
PHYSICAL PROPERTIES |
---|
Crystal Structure | Face centered cubic (fcc) |
Specific Gravity | 7.78 |
Magnetic Properties | Ferromagnetic |
ELECTRICAL PROPERTIES |
---|
Electrical Volume Resistivity | 6e-7 ohm.m |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 26.1 W/m.K |
Thermal Expansion Coefficient | 10.4 μstrain/°C |
Specific Heat | 0.46 J/g.K |
Melting Range | 1430 to 1510 °C |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
General Corrosion Status | No specific corrosion protection required |
Stress Corrosion Status | High Resistance to SCC: Table 1 Remark: Tempering between 371C and 593C shall be avoided because corrosion and stress corrosion cracking resistance is lowered. Data Quality: Design Data |
Bimetallic Corrosion | Can be connected without any restriction to: Cr, Au, Ag, Gun-metal, P-bronzes, Sn-bronzes, Ti+alloys, Ni, Monel, Inconel, Ni/Mo alloys
Can be connected in a non-controlled environment to the above and Cd, austenitic cast iron, Cu, Brasses, Al-bronzes, Si-bronzes, Au, Pt, C, Rh, Sn-Pb alloys, Sn, Pb, 300 series stainless steels Can be connected in a clean room environment to above and Al-Cu alloys Needs specific measures: All others Test:ECSS-Q-ST-70C Rev.1 Table 5.1 Data Quality: Design Data |