Data still to be completed------(Home) | |
---|---|
PRODUCT DATA of CDA 422 |
Material | CDA 422 |
General Information | Typical data from standards handbook of copper and copper alloys (Copper.org) @ Room Temperature |
Chemical Composition | Cu-12Zn-1Sn |
EXPERIENCE IN PRACTICE |
---|
Equivalent Designations | CDA422 |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 8.8 |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 124 GPa |
ELECTRICAL PROPERTIES |
---|
Electrical Volume Resistivity | 5.49e-8 ohm.m |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 130 W/m.K |
Specific Heat | 0.377 J/g.K |
Melting Range | 1020 to 1040 °C |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
Stress Corrosion Status | High Resistance to SCC: Table 1
Remark: in the 37% cold rolled condition only Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |