Data still to be completed------(Home) | |
---|---|
PRODUCT DATA of CDA 770 |
Material | CDA 770 |
General Information | Typical data from standards handbook of copper and copper alloys (CDA inc) @ Room Temperature |
Chemical Composition | Cu-18.5Ni-27%Zn |
EXPERIENCE IN PRACTICE |
---|
Equivalent Designations | C77000; CuN18Zn27; CW410J; 2.0742; NS107; CDA770; nickel-silver 55-18 |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 8.7 |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 125 GPa |
Shear Modulus | 41.7 GPa |
ELECTRICAL PROPERTIES |
---|
Electrical Volume Resistivity | 3.14e-7 ohm.m |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 29.3 W/m.K |
Thermal Expansion Coefficient | 16.7 µstrain/°C |
Specific Heat | 0.377 J/g.K |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
Stress Corrosion Status | Low Resistance to SCC: Table 3
Remark: in the annealed, 38% or 50% cold rolled condition only Remark: Requires Stress corrosion evaluation form Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |