PRODUCT DATA of CDA 917 |
Material | CDA 917 |
General Information | cast alloy Data @ Room Temperature |
Chemical Composition | Cu-12Sn-2Ni |
EXPERIENCE IN PRACTICE |
---|
Equivalent Designations | C91700; CuSn12Ni2-B; CB484K; CuSn12NI; 2.1060; CT2; CDA917 |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 8.75 |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 103 GPa |
ELECTRICAL PROPERTIES |
---|
Electrical Volume Resistivity | 1.72e-7 ohm.m |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 70.6 W/m.K |
Thermal Expansion Coefficient | 16.2 µstrain/°C |
Specific Heat | 0.377 J/g.K |
Melting Range | 851 to 1010 °C |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
Stress Corrosion Status | High Resistance to SCC: Table 1
Remark: in the 0% cold rolled condition only Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |